It is recommended to burn out the printing part at 1000~1200 oC for 1~2 hours. the final ash content is tightly related to the printing part°Øs topological structure as well as the burning condition: please ensure there is enough air blowing when burning out the part, please also ensure the print part°Øs structure is not extremely complicated (for extreme complicated structure, two-times burning may be necessary).